* All tests were performed at 25. C. 2 ک * Viscosity is performed at 25. C and 60 rpm and Spindle No. 3. 3 * To harden the resin, 0.1 g of cobalt 10% and methyl ethyl ketone peroxide of type A60 are required in the amount of 1.5 g per 100 g of resin at 25 درجه C.
For this product no file has been considered.
* All tests were performed at 25. C. 2 ک * Viscosity is performed at 25. C and 60 rpm and Spindle No. 3. 3 * To harden the resin, 0.1 g of cobalt 10% and methyl ethyl ketone peroxide of type A60 are required in the amount of 1.5 g per 100 g of resin at 25 درجه C.